Abstract
Bonding of ceramic to the alloy is essential for the longevity of porcelain fused to metal restorations. Imported alloys used now a days in processing them are not economical. So this study was conducted to evaluate and compare the bond strength of ceramic material to nickel based cost effective Nonferrous Materials Technology Development Center (NFTDC), Hyderabad and Heraenium S, Heraeus Kulzer alloy. An Instron testing machine, which has three-point loading system for the application of load onto the specimen was utilized for analyzing bond strength of both alloys. Student t test was conducted and t value obtained was 0.644, and the mean value of flexural bond strength of indigenous alloy is 81.75 with standard deviation of 12.25 and of imported alloy is 84.42 with standard deviation of 10.35, indicating that there was no significant difference between the two alloys. Due to ever increasing cost of imported non-precious alloy the need for a costeffective replacement was fulfilled by indigenous NFTDC alloy.
Author supplied keywords
Cite
CITATION STYLE
Ramesh, G., Padmanabhan, T. V., Ariga, P., Joshi, S., Bhuminathan, S., & Vijayaraghavan, V. (2013). Surface bond strength in Nickel based alloys. Journal of Indian Prosthodontist Society, 13(4), 551–554. https://doi.org/10.1007/s13191-012-0186-x
Register to see more suggestions
Mendeley helps you to discover research relevant for your work.