Activation stress for slip systems of pure magnesium single crystals in pure shear test

17Citations
Citations of this article
34Readers
Mendeley users who have this article in their library.

Abstract

With a hexagonal close packed structure, magnesium has many slip systems. Pure shear tests were carried out to evaluate their critical resolved shear stresses (CRSS). As a result, the CRSS for the basal slip was 0.7 MPa, and it was close to conventional values. When the shear stress of 40 MPa was applied in parallel to the prismatic plane, the {10l2} twin deformation occurred only, and the prismatic slip deformation did not occur.

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Cite

CITATION STYLE

APA

Fukuda, K., Koyanagi, Y., Tsushida, M., Kitahara, H., Mayama, T., & Ando, S. (2017). Activation stress for slip systems of pure magnesium single crystals in pure shear test. Materials Transactions, 58(4), 587–591. https://doi.org/10.2320/matertrans.M2016402

Readers over time

‘16‘18‘19‘20‘21‘22‘23‘24‘25036912

Readers' Seniority

Tooltip

PhD / Post grad / Masters / Doc 13

65%

Researcher 5

25%

Professor / Associate Prof. 2

10%

Readers' Discipline

Tooltip

Materials Science 14

70%

Engineering 4

20%

Agricultural and Biological Sciences 1

5%

Computer Science 1

5%

Save time finding and organizing research with Mendeley

Sign up for free
0