Fabrication of SiC Composites with Synergistic Toughening of Carbon Whisker and in Situ 3C-SiC Nanowire

1Citations
Citations of this article
6Readers
Mendeley users who have this article in their library.

This article is free to access.

Abstract

The SiC composites with synergistic toughening of carbon whisker and in situ 3C-SiC nanowire have been fabricated by hot press sinter technology and annealed treatment technology. Effect of annealed time on the morphology of SiC nanowires and mechanical properties of the Cw/SiC composites was surveyed in detail. The appropriate annealed time improved mechanical properties of the Cw/SiC composites. The synergistic effect of carbon whisker and SiC nanowire can improve the fracture toughness for Cw/SiC composites. The vapor-liquid-solid growth (VLS) mechanism was proposed. TEM photo showed that 3C-SiC nanowire can be obtained with preferential growth plane ({111}), which corresponded to interplanar spacing about 0.25 nm.

Cite

CITATION STYLE

APA

Yunlong, Z., Yumin, Z., Ming, H., & Jinping, L. (2016). Fabrication of SiC Composites with Synergistic Toughening of Carbon Whisker and in Situ 3C-SiC Nanowire. Advances in Materials Science and Engineering, 2016. https://doi.org/10.1155/2016/2565137

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free