Abstract
This study investigates the effects of different post-weld heat treatments (PWHT) on the mechanical properties and microstructure of ASTM 335 Gr P91 martensitic steel, commonly used in boiler applications. Mechanical tests were conducted at room temperature, 300°C, and 600°C. Two PWHT conditions were applied: (i) PWHT-1, involving a 300°C isothermal treatment followed by heating to 770°C, and (ii) PWHT-2, following the same profile but without cooling to room temperature after the initial isothermal step. The resulting microstructure exhibited martensitic features, with a gradient of prior austenite grain boundaries in the heat-affected zone (HAZ) and δ-ferrite formation in the fusion zone (FZ), reducing toughness. Ultimate tensile strength decreased with increasing temperature, ranging from 675–750 MPa (RT), 525–615 MPa (300°C), and 375–440 MPa (600°C). Elongation was highest at 600°C (BM: 25–30%, FZ: 8–20%), decreasing at room temperature (BM: 20–25%, FZ: 2–12%). Toughness tests showed crack propagation across BM, HAZ, and FZ, with the lowest energy absorption in FZ (0.05–0.4 mm, 12–50 J). At 600°C, toughness decreased in BM and HAZ but increased in FZ, suggesting a change in deformation mechanisms at elevated temperatures.
Author supplied keywords
Cite
CITATION STYLE
Bento, E. A. P., Torres, E. A., Chemin, A. E. A., Dos Santos Maciel, C. I., Caselatto, A. L., Ruchert, C. O. F. T., & Avila, J. A. (2025). Influence of Post-Weld Heat Treatment on the Mechanical Properties and Microstructure of a Seamless Pipe of an ASTM A335 Gr P91 Steel. Materials Research, 28. https://doi.org/10.1590/1980-5373-MR-2024-0544
Register to see more suggestions
Mendeley helps you to discover research relevant for your work.