This study examines the phase stability of perovskite SrTiO3 in Na2SO4 + 50 wt.% V2O5 and Na2SO4 + 10 wt.% NaCl environments at 900°C. Hot corrosion results show the formation of Sr2VO4, SrV2O6, and SrTiV5O11 phases in Na2SO4 + 50 wt.% V2O5 environment and Sr3Ti2O7, Na4TiO4, and TiO2 phases in Na2SO4 + 10 wt.% NaCl environment. Morphological observations revealed the austerity of hot corrosion attack on SrTiO3. The Sr2+ ions leached out from SrTiO3 and reacted with corrosive environments. These observations clearly indicate the destabilization of SrTiO3 in both environments.