Leaching of chalcopyrite in acidified nitrate using seawater-based media

42Citations
Citations of this article
43Readers
Mendeley users who have this article in their library.

Abstract

The leaching of copper from industrial copper ore with 4.8 wt % chalcopyrite by acidified nitrate with seawater based media was investigated. Water quality (pure water and seawater), temperature (25–70 °C), reagent concentration, and nitrate type (sodium and potassium) were studied variables. Leaching conditions were: 100 g ore/1 L solution; P80 of 62.5 µm; 400 rpm and leaching time, varying between 3 and 7 days. Nitrates in sulfuric acid are known to be good oxidants for sulfide ores. This study showed that up to 80 wt % copper could be extracted at 45 °C in 7 days. In the absence of nitrate, under the same leaching conditions, only a 28 wt % copper extraction was achievable. The extraction rate increased to 97.2 wt % when leach temperature was increased to 70 °C in nitrate-chloride-acid media. The presence of chloride ions also increased the copper extraction rate. The copper extraction achieved in seawater systems were higher than in water systems under the same leaching conditions (increased by an average of 18 wt %). This effect can be attributable to the contribution of chloride that increases proton (H+) activity.

Cite

CITATION STYLE

APA

Hernández, P. C., Taboada, M. E., Herreros, O. O., Graber, T. A., & Ghorbani, Y. (2018). Leaching of chalcopyrite in acidified nitrate using seawater-based media. Minerals, 8(6). https://doi.org/10.3390/min8060238

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free