Enhancement of oxygen reduction and mitigation of ionomer dry-out using insoluble heteropoly acids in intermediate temperature polymer-electrolyte membrane fuel cells

5Citations
Citations of this article
15Readers
Mendeley users who have this article in their library.

Abstract

The use of Cs0.5H0.5PW12O40 insoluble salt as a superacid promoter in the catalyst layer of a polymer electrolyte membrane fuel cell (PEMFC) has been investigated. An increase of performance has been recorded at intermediate temperatures (110-130 °C) and under low relative humidity (R.H.). The promoter appears to mitigate the ionomer dry-out effects in the catalytic layer and produces an increase of the extent of the catalyst-electrolyte interface as demonstrated by cyclic voltammetry analysis. These effects are also corroborated by a significant decrease of polarization resistance at intermediate temperatures. Such characteristics have been demonstrated for a conventional membrane-electrode assembly based on a Pt-Co alloy and a Nafion 115 membrane.

Cite

CITATION STYLE

APA

Stassi, A., Gatto, I., Saccà, A., Baglio, V., & Aricò, A. S. (2015). Enhancement of oxygen reduction and mitigation of ionomer dry-out using insoluble heteropoly acids in intermediate temperature polymer-electrolyte membrane fuel cells. Energies, 8(8), 7805–7817. https://doi.org/10.3390/en8087805

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free