Dielectric properties of bismuth titanate ceramics containing SiO2 and Nd2O3 as additives

  • Slavov S
  • Krapchanska M
  • Kashchieva E
  • et al.
N/ACitations
Citations of this article
6Readers
Mendeley users who have this article in their library.

Abstract

Bismuth-titanate ceramics containing SiO2 and Nd2O3 as additives are synthesized by melt quenching method in the system Bi2O3-TiO2-Nd2O3-SiO2 in the temperature range of 1250-1500 ?C. The phase composition of the obtained materials is determined by X-ray diffraction analysis and energy dispersive spectroscopy. Using scanning electron microscopy different microstructures are observed in the samples depending on the composition. Different values of conductivity, dielectric losses and relative permittivity are obtained depending on the composition. It is established that all investigated samples are dielectric materials with conductivity between 10-9 and 10-13 (??cm)-1 at room temperature, dielectric permittivity from 1000 to 3000 and dielectric losses tg? between 0.0002 and 0.1.nema

Cite

CITATION STYLE

APA

Slavov, S., Krapchanska, M., Kashchieva, E., Parvanov, S., & Dimitriev, Y. (2012). Dielectric properties of bismuth titanate ceramics containing SiO2 and Nd2O3 as additives. Processing and Application of Ceramics, 6(3), 117–122. https://doi.org/10.2298/pac1203117s

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free