Comparative study of ceramic-to-metal bonding

11Citations
Citations of this article
31Readers
Mendeley users who have this article in their library.

Abstract

Dentists and technicians have used dental ceramics associated with different types of alloys without taking into account the characteristics of compatibility of these materials. Knowing the properties of the alloy and ceramic used in metal/ceramic restorations is a key factor for treatment success. The purpose of this study was to evaluate the bond strength of a palladium-silver alloy (Pors-on 4) to 3 ceramics (Ceramco, Noritake and Vita VMK-68) using shear forces at the metal-ceramic interface. A stainless steel cylindrical matrix was used for preparation of the metal dies, application of ceramic and shear strength testing. Thirty palladium-silver alloy cylinders received two layers of opaque and two layers of body porcelain, and shear tests were performed in a universal testing machine at a cross-head speed of 0.5 mm/min. Shear bond strength means (in MPa) were: 28.21(Ceramco), 28.96 (Noritake) and 24.11 (Vita VMK-68). One-way ANOVA did not show statistically significant differences (p>0.05) among the materials. The results of this study indicate that the three evaluated ceramic systems are suitable to be used in combination with the tested palladium-silver alloy.

Cite

CITATION STYLE

APA

Scolaro, J. M., Pereira, J. R., do Valle, A. L., Bonfante, G., & Pegoraro, L. F. (2007). Comparative study of ceramic-to-metal bonding. Brazilian Dental Journal, 18(3), 240–243. https://doi.org/10.1590/S0103-64402007000300012

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free