The microstructural evolution during refill friction stir spot welding of an AlMgSc alloy was studied. The primary texture that developed in all regions, with the exception of the weld center, was determined to be 〈110〉 fibers and interpreted as a simple shear texture with the 〈110〉 direction aligned with the shear direction. The material flow is mainly driven by two components: the simple shear acting on the horizontal plane causing an inward-directed spiral flow and the extrusion acting on the vertical plane causing an upward-directed or downward-directed flow. Under such a complex material flow, the weld center, which is subjected to minimal local strain, is the least recrystallized. In addition to the geometric effects of strain and grain subdivision, thermally activated high-angle grain boundary migration, particularly continuous dynamic recrystallization, drives the formation of refined grains in the stirred zone.

Cite

CITATION STYLE

APA

Shen, J., Lage, S. B. M., Suhuddin, U. F. H., Bolfarini, C., & dos Santos, J. F. (2018). Texture Development and Material Flow Behavior During Refill Friction Stir Spot Welding of AlMgSc. Metallurgical and Materials Transactions A: Physical Metallurgy and Materials Science, 49(1), 241–254. https://doi.org/10.1007/s11661-017-4381-6

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free