Abstract
The paper presents the results of a study on the corrosion behaviour of copper (EN CW004A) in five possible phase change materials (PCMs): magnesium nitrate hexahydrate pure and with an addition of Mg(OH) 2 (0.5 wt. %) or Sr(OH) 2 (0.5 wt. %) at 90 °C, calcium nitrate tetrahydrate at 50 °C and a mixture of magnesium nitrate hexahydrate and calcium nitrate tetrahydrate (1:1 mass ratio) at 72 °C. The corrosion rate of copper samples is low except for the use of Mg(NO 3 ) 2 · 6H 2 O with/without an addition of Mg(OH) 2 . The lowest corrosion rate was observed for the mixture Mg(NO 3 ) 2 · 6H 2 O—Ca(NO 3 ) 2 · 4H 2 O (1:1), and it was ca six times lower than that of pure magnesium nitrate hexahydrate.
Cite
CITATION STYLE
Danielik, V., Šoška, P., & Felgerová, K. (2016). Corrosive effects of nitrate-containing phase change materials used with copper. Acta Chimica Slovaca, 9(2), 75–83. https://doi.org/10.1515/acs-2016-0013