High Temperature Testing of NMC/Graphite Cells for Rapid Cell Performance Screening and Studies of Electrolyte Degradation

  • Taskovic T
  • Eldesoky A
  • Song W
  • et al.
27Citations
Citations of this article
62Readers
Mendeley users who have this article in their library.

This article is free to access.

Abstract

LiNi 0.5 Mn 0.3 Co 0.2 O 2 /graphite cells with two different electrolytes underwent charge-discharge cycling at 70 °C. The 70 °C condition reduced the time it took for cells to lose significant capacity. Studies of the changes to the electrolyte after cycling by gas chromatography/mass spectrometry (GC/MS) and by Nuclear Magnetic Resonance spectroscopy (NMR) suggest that the same processes which cause cell failure and electrolyte degradation at 40 °C and 55 °C occur at 70 °C, only at an accelerated rate. Transition metal dissolution from the positive electrode was tracked using X-ray fluorescence studies of the negative electrode after testing. Based on the confidence obtained that the same degradation processes were occurring; advanced graphites were screened in NMC811/graphite cells at 70 °C. Differences in cell lifetime were apparent in weeks at 70 °C while the same differences took much longer to observe at 40 °C. It is our opinion that elevated temperature testing of Li-ion cells at 70 °C is a viable rapid screening technique for advanced electrolytes and advanced electrode materials.

Cite

CITATION STYLE

APA

Taskovic, T., Eldesoky, A., Song, W., Bauer, M., & Dahn, J. R. (2022). High Temperature Testing of NMC/Graphite Cells for Rapid Cell Performance Screening and Studies of Electrolyte Degradation. Journal of The Electrochemical Society, 169(4), 040538. https://doi.org/10.1149/1945-7111/ac6453

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free