Abstract

Objective: To evaluate fracture strength of veneered translucent zirconium dioxide crowns designed with different porcelain layer thicknesses. Materials and Methods: Sixty crowns, divided into six groups of 10, were used in this study. Groups were divided according to different thicknesses of porcelain veneer on translucent zirconium dioxide cores of equal thickness (0.5 mm). Porcelain thicknesses were 2.5, 2.0, 1.0, 0.8, 0.5 and 0.3 mm. Crowns were artificially aged before loaded to fracture. Determination of fracture mode was performed using light microscope. Results: Group 1.0 mm showed significantly (p.05) in fracture loads among groups 1.0, 0.8 and 0.5 mm (mean 1540, 1313 and 1286 N). There were significantly (p

Cite

CITATION STYLE

APA

Bakitian, F., Seweryniak, P., Papia, E., Larsson, C., & Vult von Steyern, P. (2017). Fracture strength of veneered translucent zirconium dioxide crowns with different porcelain thicknesses. Acta Biomaterialia Odontologica Scandinavica, 3(1), 74–83. https://doi.org/10.1080/23337931.2017.1403288

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free