The degree of tissue reaction of 4 nonabsorbable suture materials (linen, nylon, polymerized caprolactum and polypropylene) implanted into health skin of 8 horses was clinically and histologically evaluated. Cutaneous oedema and absence or presence of the exudation were clinically evaluated 5 and 10 days following suture material implantation. Biopsies were taken to histologically evaluate tissue reaction at 10 days. The results obtained showed that linen caused more oedema by the 5 th day, whereas the nylon and caprolactum had less oedema on the 10 th day. With respect to the presence or absence of exudation, nylon was the only material which did not show exudation by the 5th day in any of the 8 samples, but on the 10 th day, neither the nylon, caprolactum or polypropylene showed exudation, except one horse that showed exudation for all suture materials. The histological evaluation showed that nylon and caprolactum caused less tissue reaction. In conclusion, linen was found to have a higher degree of tissue reaction in the present study, and nylon although similar to caprolactum and polypropylene in terms of tissue reaction, caused less cases of exudate than the other suture materials used. © 2006 Facultad de Ciencias Veterinarias, Universidad Austral de Chile.

Cite

CITATION STYLE

APA

Maldonado, F., Muñoz, L., Quezada, M., Briones, M., & Urrutia, P. (2006). Reacción tisular a materiales de sutura no absorbibles en piel de equinos. Archivos de Medicina Veterinaria, 38(1), 63–67. https://doi.org/10.4067/s0301-732x2006000100009

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free