Abstract

From the research to determine the thermoelectric properties and crystal structure of SbTe material synthesized by ball mill at 350 rpm for 10 h and sintered with hot press. The hot press method was varied at the time of hot press for 1, 2 and 3 h. The hot press temperature is 400 °C with a pressure of 25MPa. Then all materials were tested by XRD and ZEM 3. Based on the XRD test performed, all materials had hexagonal crystal structures. From ZEM 3 measurement known that the best thermoelectric properties value is in sample 3 which has an electrical resistivity 0.35 mΩcm at 331 K, Seebeck coefficient 147 μV/K at 473 K and power factor 4.53 mW/mK2 at 331 K.

Cite

CITATION STYLE

APA

Najma, Z. S., Singsoog, K., Melania, S. M., & Seetawan, T. (2020). Thermoelectric Properties of SbTe. In Journal of Physics: Conference Series (Vol. 1428). Institute of Physics Publishing. https://doi.org/10.1088/1742-6596/1428/1/012008

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free