The presence of a Fe-FeAl2 O4 structure over an Fe-Al2 O3 catalysts is demonstrated to be vital for the catalytic methane decomposition (CMD) activity. After H2 reduction at 750 °C, Fe-Al2 O3 prepared by means of a fusion method, containing 86.5 wt % FeAl2 O4 and 13.5 wt % Fe(0) , showed a stable CMD activity at 750 °C for as long as 10 h.

Cite

CITATION STYLE

APA

Zhou, L., Enakonda, L. R., Saih, Y., Loptain, S., Gary, D., Del-Gallo, P., & Basset, J. M. (2016). Catalytic Methane Decomposition over Fe-Al2 O3. ChemSusChem, 9(11), 1243–1248. https://doi.org/10.1002/cssc.201600310