Press-fit stability of uncemented hemispheric acetabular components: A comparison of three porous coating systems

50Citations
Citations of this article
35Readers
Mendeley users who have this article in their library.

Abstract

Cementless acetabular components require good initial fixation to allow bony in-growth. The initial press-fit stability, important for designs that do not rely on supplemental fixation, was examined for three designs with different porous coating systems: beads, fiber mesh, and plasma spray. The ability to withstand tangential loads was determined (maximum rim loads: 122-1730 N). The plasma-sprayed acetabular cups withstood the greatest tangential load within the specified range of motion of 150 μm (P<0.01). Differences in surface preparation of titanium acetabular cups may significantly affect the initial stability of the implants in rim loading.

Cite

CITATION STYLE

APA

Markel, D. C., Hora, N., & Grimm, M. (2002). Press-fit stability of uncemented hemispheric acetabular components: A comparison of three porous coating systems. International Orthopaedics, 26(2), 72–75. https://doi.org/10.1007/s00264-001-0314-4

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free