Studies on thermal decomposition of phenol binder using TG/DTG/DTA and FTIR-DRIFTS techniques in temperature range 20–500 °C

25Citations
Citations of this article
24Readers
Mendeley users who have this article in their library.
Get full text

Abstract

This paper presents results of thermoanalytical and structural research on phenolic binder used in foundry for the preparation of moulding sand. The binder has been prepared based on resole type phenolic resin with the addition of ester hardener. The aim of the study was to determine the structural changes taking place in the phenolic binder under the influence of temperature. Results show that in the investigated range of temperatures, phenolic binder exhibits three exothermic thermal effects accompanying the decomposition process. The test results using the Diffuse Reflectance Infrared Fourier Transform Spectroscopy (DRIFTS) technique show that the addition of a hardener stabilizes the binder structure within methylene bridges. The reduction in the reaction rate observed in the DTA curve at about 330 °C can be associated with the formation of gaseous products by decomposition of the binder or, as suggested by the literature data, the formation of triple bonds and CN-HCN groups.

Cite

CITATION STYLE

APA

Bobrowski, A., Drożyński, D., Grabowska, B., Kaczmarska, K., Kurleto-Kozioł, Ż., & Brzeziński, M. (2018). Studies on thermal decomposition of phenol binder using TG/DTG/DTA and FTIR-DRIFTS techniques in temperature range 20–500 °C. China Foundry, 15(2), 145–151. https://doi.org/10.1007/s41230-018-7035-4

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free