Manganese, iron and sulfur K edge XAFS of promoted sulfated zirconia catalysts

9Citations
Citations of this article
10Readers
Mendeley users who have this article in their library.
Get full text

Abstract

Promoted sulfated zirconia samples were prepared by the incipient wetness technique to produce isomerization catalysts which were active for the conversion of n-butane to isobutane at 338K (up to 10% conversion of 1% n-butane, 1atm., 0.25 h-1 WHSV). The local structure of Fe and Mn in promoted sulfated zirconia was investigated using fluorescence yield XAS. Spectra were taken of calcined samples, activated samples, and samples after reaction with n-butane (maximum activity and deactivated). Factor analysis reveals that the Mn K edge XANES can be described by a linear combination of the spectra of two separate components, and that the ratio of these components changes with activation of the catalyst, and during use in the n-butane isomerization reaction. The change in ratio of the Mn species during activation and reaction results in a reduction of the average Mn valence from 2.4 to 2.2. The Fe K edge XANES was not similarly affected by activation and reaction with n-butane.

Cite

CITATION STYLE

APA

Jentoft, R. E., Hahn, A., Jentoft, F. C., & Ressler, T. (2001). Manganese, iron and sulfur K edge XAFS of promoted sulfated zirconia catalysts. Journal of Synchrotron Radiation, 8(2), 563–565. https://doi.org/10.1107/S0909049500017465

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free