Comparison of the effect of proanthocyanidin surface treatments on shear bond strength of different cements

7Citations
Citations of this article
21Readers
Mendeley users who have this article in their library.

Abstract

This study aimed to compare the effect of proanthocyanidin-rich grape seed extract (Pa-rich GSE) in two different concentrations on the bond strength to dentin tissue for four different cement groups (resin cement (P), resin modified glass ionomer cement (K), calcium aluminate glass ionomer cement (C), glass ionomer cement (G)). One hundred and eighty dentin surfaces of the extracted molar teeth placed on acrylic cylinders were divided into 12 groups randomly (n = 15). Each cement group was further divided into control (CP, CC, CK, CG), 6.5% Pa-rich GSE (P6.5, C6.5, K6.5, G6.5) and 12.5% Pa-rich GSE (P12.5, C12.5, K12.5, G12.5) subgroups. In accordance with the manufacturer's recommendations the cements were applied. After shear bond tests, surfaces were examined under a stereomicroscope. Median shear bond strength (in MPa) of CP, CK, CC, CG groups were 14.13, 7.05, 4.87, 3.86; for the P6.5, G6.5, C6.5, K6.5 groups they were 13.98, 13.42, 6.21, 3.27; and for the P12.5, C12.5, K12.5, G12.5 groups they were 15.08, 5.40, 3.10, 0.00, respectively. CK and K6.5 groups showed a significant difference from the K12.5 group (p < 0.05). Also, CG, G6.5 and G12.5 groups were found statistically different from each other (p < 0.05). Applied to the dentin surface, 6.5% Pa-rich GSE enhanced the bond strength of glass ionomer cements.

Cite

CITATION STYLE

APA

Atabek, S., & Nehir özden, A. (2019). Comparison of the effect of proanthocyanidin surface treatments on shear bond strength of different cements. Materials, 12(7). https://doi.org/10.3390/ma12172676

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free