Evaluation of Bioactive Properties of α and β Wollastonite Bioceramics Soaked in a Simulated Body Fluid

  • Núñez-Rodríguez L
  • Encinas-Romero M
  • Gómez-Álvarez A
  • et al.
N/ACitations
Citations of this article
33Readers
Mendeley users who have this article in their library.

Abstract

Dense natural wollastonite bioceramics (CaSiO3) were prepared by a sintering method, varying the pressing load and sintering temperature, in order to obtain different phases of wollastonite, and different physical properties in the materials. The products were characterized by TGA-DTA, XRD, FT-IR, SEM-EDS, TEM and XPS techniques. The results indicate the presence of two polymorphic phases of wollastonite, the β-wollastonite and α-wollastonite with a transition temperature of the β phase to α phase at approximately 1250˚C. These materials were soaked in a simulated body fluid (SBF) during 1, 2 and 3 weeks, to study their solubility and bioactivity. The effect of different wollastonite phases on the solubility of Ca and Si, as well as the capacity of producing layers of “newly formed apatite” on the surfaces of these materials in SBF solution were analyzed.

Cite

CITATION STYLE

APA

Núñez-Rodríguez, L. A., Encinas-Romero, M. A., Gómez-Álvarez, A., Valenzuela-García, J. L., & Tiburcio-Munive, G. C. (2018). Evaluation of Bioactive Properties of α and β Wollastonite Bioceramics Soaked in a Simulated Body Fluid. Journal of Biomaterials and Nanobiotechnology, 09(03), 263–276. https://doi.org/10.4236/jbnb.2018.93015

Register to see more suggestions