Understanding the Catalytic Deactivation upon Hydrothermal Aging at 850 °C of WO3/Fe-Cu-ZSM-5 Catalyst for Selective Catalytic Reduction of NO by NH3

3Citations
Citations of this article
6Readers
Mendeley users who have this article in their library.

Abstract

A WO3/Fe-Cu-ZSM-5 catalyst was prepared using the solid state ion exchange method (SSIE) and its performance for the Selective Catalytic Reduction of NO with NH3 (NH3-SCR of NO) was investigated. The study shows that the tungsten addition can slightly improve the high temperature catalytic activity of Fe-Cu-ZSM-5. The influence of hydrothermal aging at 850 °C for 5 h on the structural and textural properties of WO3/Fe-Cu-ZSM-5 was also studied in this paper. The XRD and FE-SEM measurements did not indicate a breakdown of the zeolite structure upon steam treatment for both aged catalysts. The aged W-base catalyst demonstrates a lower deactivation and better catalytic activity for NO reduction than the bimetallic catalyst after hydrothermal aging despite the lower acidic properties as shown by FTIR-Pyr spectroscopy owing to the presence of tungsten oxide crystallites. The “severe” stage of aging occurring in the absence of W led to the formation of copper oxide agglomerates detected using STEM and H2-TPR techniques being responsible for the deterioration of SCR activity of the aged Fe-Cu-ZSM-5.

Author supplied keywords

Cite

CITATION STYLE

APA

Jouini, H., de Marcos-Galán, A., Mejri, I., Bensouilah, R., Mhamdi, M., Blasco, T., & Delahay, G. (2022). Understanding the Catalytic Deactivation upon Hydrothermal Aging at 850 °C of WO3/Fe-Cu-ZSM-5 Catalyst for Selective Catalytic Reduction of NO by NH3. Inorganics, 10(11). https://doi.org/10.3390/inorganics10110180

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free