The deposition of pure silica layers using the Outside Vapor Deposition method has been studied. The experimental study focuses on some fabrication parameters that have to be adjusted in order to work with a target temperature optimized for deposition of pure silica compatible with large volume deposition and post-treatments. It is experimentally shown that the optimized soot porous preforms are constituted by homogeneous silica spherical particles of 100 to 110 nm in diameter and have, in this case, densities approximately equal to 0.35 g.cm-3.
CITATION STYLE
Petit, V., Le Rouge, A., Béclin, F., El Hamzaoui, H., & Bigot, L. (2010). Experimental study of SiO2 soot deposition using the outside vapor deposition method. Aerosol Science and Technology, 44(5), 388–394. https://doi.org/10.1080/02786821003671315