Abstract
The hydrogen internal friction peak in Zr50-metallic glasses (Zr50Cu50, Zr50Cu40Al10 and Zr50Cu35Al10Ni5) was studied. The hydrogen internal friction peak was shifted exponentially to lower temperatures with increasing hydrogen concentration similarly to other Zr-Cu base metallic glasses reported in the literature. The peak height increased in proportion to the square-root of hydrogen concentration. These results were discussed in the view point of the hydrogen induced structural relaxation in these metallic glasses. © 2007 The Japan Institute of Metals.
Author supplied keywords
Cite
CITATION STYLE
Mizubayashi, H., Nakamura, I., Yamagishi, K., & Tanimoto, H. (2007). Characterization of Zr-Cu base metallic glasses by means of hydrogen internal friction peak. In Materials Transactions (Vol. 48, pp. 1822–1827). https://doi.org/10.2320/matertrans.MJ200727