Effect of nitrogen impurities on the Raman line width in diamond, revisited

42Citations
Citations of this article
47Readers
Mendeley users who have this article in their library.

Abstract

The results of a high-resolution Raman scattering study of a diamond crystal with a high content of single substitutional nitrogen impurities (550 ppm) in the temperature range from 50 to 673 K are presented and compared with the data for defect-free diamond. It is established that the increase of the nitrogen concentration in diamond leads to the temperature-independent increase of the Raman line width. Analysis of the experimental data allows us to conclude that this broadening should be attributed to the defect-induced shortening of the Raman phonon lifetime. We believe that this mechanism is responsible for the increase of the Raman line width caused by most point-like defects in diamond. No pronounced effects of the nitrogen defects on the Raman line position and phonon anharmonicity are observed.

Cite

CITATION STYLE

APA

Surovtsev, N. V., & Kupriyanov, I. N. (2017). Effect of nitrogen impurities on the Raman line width in diamond, revisited. Crystals, 7(8). https://doi.org/10.3390/cryst7080239

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free