Atomic disorder of Li0.5Ni0.5O thin films caused by Li doping: Estimation from X-ray Debye-Waller factors

2Citations
Citations of this article
9Readers
Mendeley users who have this article in their library.

Abstract

Cubic type room-temperature (RT) epitaxial Li0.5Ni0.5O and NiO thin films with [111] orientation grown on ultra-smooth sapphire (0001) substrates were examined using synchrotron-based thin-film X-ray diffraction. The 1 1 and 2 2 rocking curves including six respective equivalent reflections of the Li0.5Ni0.5O and NiO thin films were recorded. The RT B 1 factor, which appears in the Debye-Waller factor, of a cubic Li0.5Ni0.5O thin film was estimated to be 1.8 (4) Å2 from its 1 1 and 2 2 reflections, even though the Debye model was originally derived on the basis of one cubic element. The corresponding Debye temperature is 281 (39) K. Furthermore, the B 2 factor in the pseudo-Debye-Waller factor is proposed. This parameter, which is evaluated using one reflection, was also determined for the Li0.5Ni0.5O thin film by treating Li0.5Ni0.5O and NiO as ideal NaCl crystal structures. A structural parameter for the atomic disorder is introduced and evaluated. This parameter includes the combined effects of thermal vibration, interstitial atoms and defects caused by Li doping using the two Debye-Waller factors.

Cite

CITATION STYLE

APA

Yang, A., Sakata, O., Yamauchi, R., Kumara, L. S. R., Song, C., Katsuya, Y., … Yoshimoto, M. (2015). Atomic disorder of Li0.5Ni0.5O thin films caused by Li doping: Estimation from X-ray Debye-Waller factors. Journal of Applied Crystallography, 48, 1896–1900. https://doi.org/10.1107/S1600576715020002

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free