Abstract
The Cs/Ru/MgO catalyst was synthesized by sequential impregnation of Ru and Cs on MgO support using Ru(NO3 )3 and CsNO3 precursors. Catalytic ammonia synthesis was carried out in a fixed-bed flow reactor using H2 and N2 as reactants. The stability of the catalyst was measured at 350◦C, 2.5 MPa gauge pressure, and SV as 1200 h−1 using the H2/N2 ratio 3 as a reactant feedstock. The Cs/Ru/MgO catalyst retained its ammonia synthesis activity while conducting experiments at mild reaction conditions of 325◦C and 350◦C. An increase in experimental temperature to 375–425◦C decreased the ammonia synthesis activity retaining only to 42% of the initial activity after 680 h of time on stream. The deformation of the catalyst’s structure, which was caused by Cs leaching and redistribution of the Ru and increased crystallinity of MgO at high-temperature conditions, was considered the plausible reason for the drastic decrease in ammonia synthesis activity.
Author supplied keywords
Cite
CITATION STYLE
Javaid, R., & Nanba, T. (2022). Stability of Cs/Ru/MgO Catalyst for Ammonia Synthesis as a Hydrogen and Energy Carrier. Energies, 15(10). https://doi.org/10.3390/en15103506
Register to see more suggestions
Mendeley helps you to discover research relevant for your work.