Abstract
This paper investigated the effect of a two-step solution heat treatment on the mechanical properties and silicon-rich phase of 332 aluminium alloy. Traditional single-step T6 solution treatment (495 °C/6. h) increased the hardness value of the alloy by 5.96%, increased the tensile strength by 20.42% and reduced the elongation by 3.97%. Two-step solution treatment of the alloy (495 °C/2. h followed by 515 °C/4. h) increased the hardness value by 6.64%, increased the tensile strength by 16.01%, and reduced the elongation by 4.67% compared to the as-cast samples. Both solution treatments were followed by hot water quenching (75-90 °C) and artificial aging at 250 °C for 4. h. The difference in mechanical properties after heat treatment can be linked to the refinement and the spheroidisation of the silicon-rich phase in the alloy. © 2010 Elsevier Ltd.
Cite
CITATION STYLE
Azmah Hanim, M. A., Chang Chung, S., & Khang Chuan, O. (2011). Effect of a two-step solution heat treatment on the microstructure and mechanical properties of 332 aluminium silicon cast alloy. Materials and Design, 32(4), 2334–2338. https://doi.org/10.1016/j.matdes.2010.12.040
Register to see more suggestions
Mendeley helps you to discover research relevant for your work.