Abstract

Workability, mechanical properties affected by cold-working and heat-treatment, and corrosion resistance were investigated for Mg-8 and 13mass%Li binary and ternary alloys containing additional elements of Al, Cu, Zn and Ag. The workability in cold-rolling was not markedly affected by the addition of third elements. The alloys containing aluminum or silver showed age-hardening. Mg-8 and 13mass%Li alloys containing 5mass% Al were hardened by the spinodal decomposition when the alloys were quenched from temperatures higher than 473K. The elongation of a Mg-8mass%Li-1mass%Ag alloy was 96.5%. Mg-8 and 13mass%Li ternary alloys showed low corrosion resistance compared with binary alloys. © 1990, The Japan Institute of Light Metals. All rights reserved.

Cite

CITATION STYLE

APA

Matsuzawa, K., Koshihara, T., Ochiai, S., & Kojima, Y. (1990). The effect of additional element on the age-hardening characteristics and properties of Mg-Li alloys. Journal of Japan Institute of Light Metals, 40(9), 659–665. https://doi.org/10.2464/jilm.40.659

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free