Abstract

The fast catalytic pyrolysis of polystyrene in the hydrocarbon medium (light and heavy cycle oil) over zeolite catalysts at 450–550 °C was investigated. The influence of reaction conditions (medium, temperature, vapor residence time, polystyrene concentration) on polymer conversion and product distribution was studied. It was found that the polymer conversion is close to 100%, while ethylbenzene, benzene, and toluene are the main products of its transformation. The maximum yield of ethylbenzene (80%) was achieved at 550 °C, vapor residence time 1–2 s, polystyrene concentration 10%, and heavy cycle oil as the medium. The influence of zeolite topology on product distribution was explored. The possible mechanism of polystyrene pyrolysis was proposed.

Cite

CITATION STYLE

APA

Dement’ev, K. I., Bedenko, S. P., Minina, Y. D., Mukusheva, A. A., Alekseeva, O. A., & Palankoev, T. A. (2023). Catalytic Pyrolysis of Polystyrene Waste in Hydrocarbon Medium. Polymers, 15(2). https://doi.org/10.3390/polym15020290

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free