Development of scientific and technological bases for application of brown coal semi coke in the technology of non- milled silicon carbide

0Citations
Citations of this article
5Readers
Mendeley users who have this article in their library.

This article is free to access.

Abstract

Thermodynamics is investigated, and the optimum temperature and time modes of carbonization of a briquetted silica fume batch- brown coal semi coke are defined. The complete carbonization of the batch in the conditions of heat treatment is achieved at a temperature of 1923 - 1973 K within 15 - 20 minutes. The conditions and indicators of the chemical enrichment of carbonization products are established. After enrichment, the carbide content is more than 90%. Silicon carbide micro-powder is obtained with a specific surface area 8000 - 9000 m2/kg.

Cite

CITATION STYLE

APA

Anikin, A. E., Galevsky, G. V., Rudneva, V. V., Nozdrin, E. V., & Galevsky, S. G. (2016). Development of scientific and technological bases for application of brown coal semi coke in the technology of non- milled silicon carbide. In IOP Conference Series: Materials Science and Engineering (Vol. 150). Institute of Physics Publishing. https://doi.org/10.1088/1757-899X/150/1/012005

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free