Magnetic properties and microstructure of FeCoNi(CuAl)0.8Snx (0 ≤ x ≤ 0.10) high-entropy alloys

26Citations
Citations of this article
27Readers
Mendeley users who have this article in their library.

Abstract

The present work exhibits the effects of Sn addition on the magnetic properties and microstructure of FeCoNi(CuAl)0.8Snx (0 ≤ x ≤ 0.10) high-entropy alloys (HEAs). The results show all the samples consist of a mixed structure of face-centered-cubic (FCC) phase and body-centered-cubic (BCC) phase. The addition of Sn promotes the formation of BCC phase, and it also affects the shape of Cu-rich nano-precipitates in BCC matrix. It also shows that the Curie temperatures (Tc) of the FCC phase and the saturation magnetization (Ms) of the FeCoNi(CuAl)0.8Snx (0 ≤ x ≤ 0.10) HEAs increase greatly while the remanence (Br) decreases after the addition of Sn into FeCoNi(CuAl)0.8 HEA. The thermomagnetic curves indicate that the phases of the FeCoNi(CuAl)0.8Snx (0 ≤ x ≤ 0.10) HEAs will transform from FCC with low Tc to BCC phase with high Tc at temperature of 600-700 K. This work provides a new idea for FeCoNi(CuAl)0.8Snx (0 ≤ x ≤ 0.10) HEAs for their potential application as soft magnets to be used at high temperatures.

Cite

CITATION STYLE

APA

Li, Z., Wang, C., Yu, L., Gu, Y., Pan, M., Tan, X., & Xu, H. (2018). Magnetic properties and microstructure of FeCoNi(CuAl)0.8Snx (0 ≤ x ≤ 0.10) high-entropy alloys. Entropy, 20(11). https://doi.org/10.3390/e20110872

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free