Effect of exhaust gas on natural stone tablets, a laboratory experiment

4Citations
Citations of this article
5Readers
Mendeley users who have this article in their library.

Abstract

8 different natural stone types were exposed to exhaust gas under laboratory conditions to assess urban stone damage. 3 cm in diameter cylindrical test specimens were made from travertine, non-porous limestone, limestone, rhyolite tuff, sandstone, andesite, granite and marble. The samples were exposed for 1, 2, 4 and 8 hours to exhaust gas that was generated by compression ignition internal combustion engine. The exhaust emission was measured. The operating conditions of the engine were documented and several parameters (weight, density, ultrasonic pulse velocity, capillary water absorption, porosity) were measured before and after exhaust gas exposure. The tests indicate that despite the deposition of soot on the surface a significant material loss was recorded at rhyolite tuff (2m%) and at andesite (1m%). The penetration depth of soot was also different for different lithologies. A correlation was found between the ultrasonic pulse velocity and density of tested stones.

Cite

CITATION STYLE

APA

Farkas, O., & Török, Á. (2019). Effect of exhaust gas on natural stone tablets, a laboratory experiment. Periodica Polytechnica Civil Engineering, 63(1), 115–120. https://doi.org/10.3311/PPci.12708

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free