Preparation method of porous dressing materials based on butyric-acetic chitin co-polyesters

13Citations
Citations of this article
16Readers
Mendeley users who have this article in their library.

Abstract

A method for obtaining highly porous materials in the form of film, based on the butyric-acetic chitin co-polyesters, containing 90% of butyryl and 10% of acetyl groups, was developed. The highly porous films, with thickness up to 0.11 mm, were obtained by two methods: (a) pouring 5% BAC 90/10 solution in ethanol on the layer of solid salts (porophor agent) which after solidification was eluted with water; (b) application of the suspension of porophor agent in BAC 90/10 solution in the solvent mixture with density similar to bulk porophor agent. In the final stage, the materials were obtained with porosity up to 95-99% and tensile strength 5 cN, which can be used as an active layer of medical dressings. The optimised procedure was used in the production of porous medical dressings (Medisorb) on an industrial scale. In the industrial method, NaCl was used as a porophor agent in the solid form and as a 3% solution in polymer. The final materials were characterised by porosity and other functional parameters at the level recommended for medical dressings. Medisorb series materials do not show in vitro cytotoxic activity.

Cite

CITATION STYLE

APA

Draczynski, Z., Kolesinska, B., Latanska, I., & Sujka, W. (2018). Preparation method of porous dressing materials based on butyric-acetic chitin co-polyesters. Materials, 11(12). https://doi.org/10.3390/ma11122359

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free