Phosphorus Partition between CaOsatd.-BaO-SiO2-FetO Slags and Liquid Iron at 1873K.

  • Nakamura S
  • Tsukihashi F
  • Sano N
N/ACitations
Citations of this article
5Readers
Mendeley users who have this article in their library.

Abstract

Unconventional, highly basic slags such as CaO bearing slags are to be used for producing high quality steel. The purpose of this study is to find out what the thermodynamic properties of CaOsatd.-BaO-SiO2-FetO slags are at steelmaking temperatures. The phosphorus partition between CaOsatd.-BaO-SiO2-FetO slags and liquid iron was measured as a function of slag composition, together with the CaO solubility. The phosphate capacity of the present system at 1873 K ranged from 1017.3 to 1020.0. BaO has been observed to be more effective than CaO for dephosphorization of steel in a thermodynamic sense. The activity coefficients of FeO and FeO1.5 have been measured and discussed in terms of the stability of orthosilicates. The FeOn(2n-3)- anion is likely to be a species of iron in the CaOsatd.-BaO-SiO2-FetO system, judging from the measurement of Fe3+/Fe2+ ratio.

Cite

CITATION STYLE

APA

Nakamura, S., Tsukihashi, F., & Sano, N. (1993). Phosphorus Partition between CaOsatd.-BaO-SiO2-FetO Slags and Liquid Iron at 1873K. ISIJ International, 33(1), 53–58. https://doi.org/10.2355/isijinternational.33.53

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free