Abstract
The present work seeks to evaluate the biocompatibility of experimental glass ionomer cements (GIC) prepared from niobium-calcium fluoro-alumino-silicate glass powder and two commercial GICs. The GICs were implanted into the subcutaneous connective tissue of sixty rats. The rats were sacrificed during four varying time periods: 7, 15, 30, and 60 days and histopathological examinations were then performed. The Kruskal-Wallis test was performed to evaluate any significant differences between the materials. Additionally, multiple comparisons of the mean rank were also carried out using the Dunn test (p<0.05). No significant differences were observed that one GIC was superior to the other. The tissue response for all of the GICs tested was similar in all the periods examined.
Author supplied keywords
Cite
CITATION STYLE
Boaventura, J. M. C., Bertolini, M. J., Padovani, G. C., de Oliveira J́nior, M. R. B., Zaghete, M. A., de Oliveira, O. B., & de Andrade, M. F. (2012). Tissue response to experimental dental cements prepared from a modified power glass composition. Dental Materials Journal, 31(4), 583–592. https://doi.org/10.4012/dmj.2011-235
Register to see more suggestions
Mendeley helps you to discover research relevant for your work.