Correction to: Network-Strengthened Ti-6Al-4V/(TiC+TiB) Composites: Powder Metallurgy Processing and Enhanced Tensile Properties at Elevated Temperatures (Metallurgical and Materials Transactions A, (2019), 50, 8, (3629-3645), 10.1007/s11661-019-05244-7)

3Citations
Citations of this article
6Readers
Mendeley users who have this article in their library.
Get full text

Abstract

In the original article, there is an error in Figure 1. The unit of Specific strength should be MPa/(g•cm-3). Following is the corrected figure:

Cite

CITATION STYLE

APA

Wei, S., Huang, L., Li, X., Jiao, Y., Ren, W., & Geng, L. (2020, March 1). Correction to: Network-Strengthened Ti-6Al-4V/(TiC+TiB) Composites: Powder Metallurgy Processing and Enhanced Tensile Properties at Elevated Temperatures (Metallurgical and Materials Transactions A, (2019), 50, 8, (3629-3645), 10.1007/s11661-019-05244-7). Metallurgical and Materials Transactions A: Physical Metallurgy and Materials Science. Springer. https://doi.org/10.1007/s11661-019-05606-1

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free