Tuning the Properties of Ester-Based Degradable Polymers by Inserting Epoxides into Poly(ϵ-caprolactone)

6Citations
Citations of this article
2Readers
Mendeley users who have this article in their library.
Get full text

Abstract

A series of ester-ether copolymers were obtained via the reaction between α,ω-dihydroxyl poly(ϵ-caprolactone) (PCL) and ethylene oxide (EO) or monosubstituted epoxides catalyzed by strong phosphazene bases. The two types of monomeric units were distributed in highly random manners due to the concurrence of epoxide ring-opening and fast transesterification reactions. The substituent of epoxide showed an interesting bidirectional effect on the enzymatic degradability of the copolymer. Compared with PCL, copolymers derived from EO exhibited enhanced hydrophilicity and decreased crystallinity which then resulted in higher degradability. For the copolymers derived from propylene oxide and 1,2-butylene oxide, the hydrophobic alkyl pendant groups also allowed lower crystallinity of the copolymers thus higher degradation rates. However, further enlarging the pendant groups by using styrene oxide or 2-ethylhexyl glycidyl ether caused a decrease in the degradation rate, which might be ascribed to the higher bulkiness hindering the contact of ester groups with lipase.

Cite

CITATION STYLE

APA

Hu, S., Liu, L., Li, H., Pahovnik, D., Hadjichristidis, N., Zhou, X., & Zhao, J. (2023). Tuning the Properties of Ester-Based Degradable Polymers by Inserting Epoxides into Poly(ϵ-caprolactone). Chemistry - An Asian Journal, 18(1). https://doi.org/10.1002/asia.202201097

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free