This study aimed to evaluate the effect of a novel bioactive glass (BAG)-containing dentin adhesive on the permeability of demineralized dentin. Bioactive glass (85% SiO2, 15% CaO) was fabricated using the sol-gel process, and two experimental dentin adhesives were prepared with 3 wt% silica (silica-containing dentin adhesive; SCA) or BAG (BAG-containing dentin adhesive; BCA). Micro-tensile bond strength (µTBS) test, fracture mode analysis, field-emission scanning electron microscopy (FE-SEM) analysis of adhesive and demineralized dentin, real-time dentinal fluid flow (DFF) rate measurement, and Raman confocal microscopy were performed to compare SCA and BCA. There was no difference in µTBS between the SCA and BCA (p > 0.05). Multiple precipitates were evident on the surface of the BCA, and partial occlusion of dentinal tubules was observed in FE-SEM of BCA-approximated dentin. The DFF rate was reduced by 50.10% after BCA approximation and increased by 6.54% after SCA approximation. Raman confocal spectroscopy revealed an increased intensity of the hydroxyapatite (HA) peak on the dentin surface after BCA application. The novel BAG-containing dentin adhesive showed the potential of both reducing dentin permeability and dentin remineralization.
CITATION STYLE
Kim, H. J., Jang, J. H., Woo, S. U., Choi, K. K., Kim, S. Y., Ferracane, J. L., … Kim, D. S. (2021). Effect of novel bioactive glass-containing dentin adhesive on the permeability of demineralized dentin. Materials, 14(18). https://doi.org/10.3390/ma14185423
Mendeley helps you to discover research relevant for your work.