The structure and properties of 5% Cr-0.5% Mo steel welded joints after natural ageing and post-weld heat treatment

4Citations
Citations of this article
8Readers
Mendeley users who have this article in their library.

Abstract

The article deals with the ageing and heat treatment influence on operational reliability of 5% Cr-0.5% Mo steel welded joints and pipeline elements. Separate components of the pipelines in the refineries are manufactured from chrome-molybdenum 5% Cr-0.5% Mo alloy steel. Reduction of internal stresses in chrome-molybdenum steel welded joints can be provided only by thermal treatment. Other methods of stress relieving are not acceptable for these steels. Presented materials analyses the impact of heat treatment on the microstructure and operational reliability of this steel. The objects of research are heat-treated welded joints of piping elements operated at high temperature for an extensive period of time, where degradation of mechanical properties has been observed. When value of the heat treatment temperature or time are exceeded, the structure degradation process is taking place, carbides coagulate within the boundaries of ferrite grains, they form coarse carbide colonies combined into long chains. Mechanical properties - tensile strength and impact strength decrease. Detailed analysis of these objects and the interpretation of the received results allow to select the most appropriate heat treatment parameters for the investigated steel structures.

Cite

CITATION STYLE

APA

Kumšlytis, V., Skindaras, R., & Valiulis, A. V. (2012). The structure and properties of 5% Cr-0.5% Mo steel welded joints after natural ageing and post-weld heat treatment. Medziagotyra, 18(2), 119–122. https://doi.org/10.5755/j01.ms.18.2.1911

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free