Study of the Non-Isothermal Crystallization Kinetics of Lithium Disilicate Glass Ceramic

7Citations
Citations of this article
5Readers
Mendeley users who have this article in their library.
Get full text

Abstract

Abstract: The glass ceramic with the crystals of lithium disilicate Li2O · 2SiO2 (LS2) as the main crystal phase is one of the prospective materials in the field of restorative dentistry. In this study, the crystallization kinetics of LS2 glass ceramic obtained from the base glass of the system SiO2–Li2O–Al2O3–K2O–P2O5 were investigated by the non-isothermal method using differential thermal analysis at four different heating rates. The DTA curves showed different exothermic crystallization peaks over the temperature ranges of 645–683 and 807–845°C. The lithium metasilicate, Li2O · SiO2 (LS), and the lithium disilicate, crystallized over these respective temperature ranges, was established by XRD technique. The crystallization kinetic parameters were calculated by the Kissinger plot and Augis-Bennett equations for non-isothermal analysis. The calculated activation energy of crystal growth, EC1= 236 kJ/mol, EC2 = 340 kJ/mol, and the Avrami parameters, n1 = 1.46–1.67, n2 = 2.73–2.91, together with the results from SEM observations, indicated that the crystallization mechanism of LS was substantial surface crystallization while the crystallization mechanism of LS2 was dominant bulk crystallization. The calculated activation energy of glass transition was also determined EV = 516 kJ/mol.

Cite

CITATION STYLE

APA

Huynh Ngoc Minh, Vuong, B. X., & Minh, D. Q. (2018). Study of the Non-Isothermal Crystallization Kinetics of Lithium Disilicate Glass Ceramic. Glass Physics and Chemistry, 44(6), 524–530. https://doi.org/10.1134/S108765961901005X

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free