Influence of temperature, basiscity and particle size on MnO reduction

8Citations
Citations of this article
6Readers
Mendeley users who have this article in their library.

Abstract

The aim of this work is to study MnO reduction by solid carbon. The influence of size of carbon particles, slag basicity, and bath temperature on MnO reduction was investigated. Fine Manganese ore particles were used as a source of MnO. Three sizes of carbon particles were used; 0.230 mm, 0.162 mm and 0.057 mm, binary basicity of 1 and 1.5 and temperatures of 1550, 1550 and 1600°C. Curves were drawn for Mn content in the bath as a function of time and temperature for the several studied parameters. The MnO reduction rates were determined using these data. © 2011 The Japan Institute of Metals.

Cite

CITATION STYLE

APA

De Oliveira, J. R., Vieira, E. A., Espinosa, D. C. R., & Tenório, J. A. S. (2011). Influence of temperature, basiscity and particle size on MnO reduction. In Materials Transactions (Vol. 52, pp. 1200–1205). https://doi.org/10.2320/matertrans.M2011007

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free