Preparation of composites with licopo4 electrode and liti2(po4)3 electrolyte for bulk-type all-solid-state lithium batteries

8Citations
Citations of this article
25Readers
Mendeley users who have this article in their library.

Abstract

All-solid-state cells with LiCoPO4 (LCP) active material with high redox potential of 4.8V (vs. Li+/Li) were fabricated and the cells operated as a lithium secondary battery at room temperature. The composite electrodes of LCP active material and LiTi2(PO4)3 (LTP) electrolyte with large contact area were synthesized in the media of oleic acid and paraffin wax by heat treatment at 700°C. The prepared LCP-LTP-Acetylene black (AB) composites were applied to electrochemical cells with a conventional organic liquid electrolyte and a sulfide solid electrolyte. The all-solid-state cells using the positive electrode composed of the LCP-LTP-AB composite and the sulfide electrolyte showed the initial discharge capacity of 50mAhg?1 at 4.8V (vs. Li+/Li). The cells using the electrodes without LTP and the sulfide electrolyte were difficult to operate, suggesting that formation of close contacts between LCP and LTP, and additional ion conduction paths to LCP-LTP particles are effective in increasing capacities in all-solid-state cells.

Cite

CITATION STYLE

APA

Harada, R., Aso, K., Hayashi, A., & Tatsumisago, M. (2015). Preparation of composites with licopo4 electrode and liti2(po4)3 electrolyte for bulk-type all-solid-state lithium batteries. In Electrochemistry (Vol. 83, pp. 898–901). Electrochemical Society of Japan. https://doi.org/10.5796/electrochemistry.83.898

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free