Abstract

Objective: To compare the bond strength of porcelain to enamel and dentin preparations finished with either ultrasonic instruments or diamond burs, with or without acid etching. Materials and Methods: A total of 140 extracted bovine incisor teeth were divided into two groups, enamel and dentin. A split tooth model was employed: each tooth having a randomly allocated combination of diamond burs, ultrasonic instrument, etching, and no etching treatments on their labial surface. Lithium disilicate glass ceramic specimens were bonded to the prepared surfaces and tensile testing was carried out. Force was applied to failure, and linear mixed models were used to analyze the data. Results: Etching increased the bond strength of the dentin samples by 7.63 MPa (P < 0.001). When bonding to dentin, ultrasonic instrument preparation produced a 2.88 MPa greater bond strength compared to burs (P < 0.001). Conclusion: Ultrasonic preparation produced greater bond strengths compared to rotary instruments. Etching improved the bond strength of all preparations, with enamel having consistently greater bonding values than dentin.

Author supplied keywords

Cite

CITATION STYLE

APA

Chew, D., Bennani, V., Aarts, J. M., Chandler, N., Gray, A., & Lowe, B. (2019). Bonding strengths to porcelain: An in vitro study of ultrasonic and conventional tooth preparation and etching. Journal of Conservative Dentistry, 22(1), 76–81. https://doi.org/10.4103/JCD.JCD_302_18

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free