Effect of the Pt buffer layer on perpendicular exchange bias based on collinear/non-collinear coupling in a Cr2O3/Co 3Pt interface

13Citations
Citations of this article
14Readers
Mendeley users who have this article in their library.
Get full text

Abstract

In this study, we fabricated a Cr2O3 (0001) film without and with a Pt buffer layer and investigated its effect on perpendicular exchange coupling in a Cr2O3/Co3Pt interface. The results showed that the exchange bias field (μ0Hex) and blocking temperature (TB) of a Cr2O3 film without and with Pt were very different. The Cr2O3 film without Pt had a lower μ0Hex of 176 Oe and a lower TB of 75 K, whereas that with Pt had a higher μ0H ex of 436 Oe and a higher TB of 150 K. We discussed this difference in μ0Hex and TB values based on collinear/non-collinear coupling in a ferromagnetic and antiferromagnetic interface using Meiklejohn and Beans exchange anisotropy model. © 2013 American Institute of Physics.

Cite

CITATION STYLE

APA

Ashida, T., Sato, Y., Nozaki, T., & Sahashi, M. (2013). Effect of the Pt buffer layer on perpendicular exchange bias based on collinear/non-collinear coupling in a Cr2O3/Co 3Pt interface. In Journal of Applied Physics (Vol. 113). https://doi.org/10.1063/1.4797472

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free