Fabrication and characterization of Ti3SiC2-SiC nanocomposite by in situ reaction synthesis of TiC/Si/Al powders

10Citations
Citations of this article
9Readers
Mendeley users who have this article in their library.
Get full text

Abstract

The microstructure and mechanical properties of Ti3SiC 2-SiC nanocomposite fabricated by in situ hot pressing (HP) synthesis process were studied. The results show that dense Ti3SiC 2-SiC composite contained minor TiSi2 obtained by hot sintering at 1350°C for 1 h. The average grain size of Ti 3SiC2 was 4 μm in length, and the size of SiC grains is about 100 nm. With its fine microstructure, the Ti3SiC 2-SiC nanocomposite shows good mechanical properties. © Indian Academy of Sciences.

Cite

CITATION STYLE

APA

Liang, B., Wang, M., Li, X., & Mu, Y. (2011). Fabrication and characterization of Ti3SiC2-SiC nanocomposite by in situ reaction synthesis of TiC/Si/Al powders. Bulletin of Materials Science, 34(7), 1309–1311. https://doi.org/10.1007/s12034-011-0320-0

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free