Optimization of Selective Hydrometallurgical Tantalum Recovery from E-Waste Using Zeolites

3Citations
Citations of this article
12Readers
Mendeley users who have this article in their library.

This article is free to access.

Abstract

To protect future high-tech metal demand, a selective and efficient recovery method for tantalum from a tantalum-rich e-waste component sample was developed. Ultrasound-assisted digestion of the component sample was optimized, and the highest dissolution rate was achieved using a mixture of 8 mol/L H2SO4 and HF at a temperature of 60 °C. The determined amount of tantalum was as high as 11 000 ± 1000 mg/kg, which results in a high potential for recyclable tantalum. The other major elements of this complex e-waste fraction were silicon, iron, aluminum, and tin. Efficient recovery of tantalum from the leachate was performed using the zeolite material ZSM-5. Extremely high selectivity and a recovery rate of over 98% were obtained. In terms of adsorption efficiency, selectivity, and durability of the material, optimal adsorption was obtained using the diluted sample at 0.5 mol/L of H2SO4. The adsorption capacity of ZSM-5 for tantalum was determined to be 10.5 ± 0.6 mg/g, and tantalum was selectively eluted with 1:4 diluted ethanolamine with a yield of 87.2 ± 1.5%.

Cite

CITATION STYLE

APA

Koskinen, J., Frimodig, J., Samulinen, M., Tiihonen, A., Siljanto, J., Haukka, M., & Väisänen, A. (2024). Optimization of Selective Hydrometallurgical Tantalum Recovery from E-Waste Using Zeolites. ACS Omega, 9(13), 14947–14954. https://doi.org/10.1021/acsomega.3c08907

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free