Abstract
The ingot and fast-cooling Sm2Co17 alloys were fabricated by arc-melting and suction casting methods, respectively. Magnetic properties of the fast-cooling Sm2Co17 alloy are enhanced than the ingot samples. The fast-cooling alloy with a diameter of 6mm has a high coercivity of 16.47kOe at room temperature. Moreover, the fast-cooling samples show a better performance than the ingot and commercial alloy, a high coercovity can be maintained below 500 °C and remain 70% of the value when temperature increased to 600°C. © Published under licence by IOP Publishing Ltd.
Cite
CITATION STYLE
Feng, H., Pan, W., Li, A., Yu, R., & Li, W. (2011). Sm2Co17 alloy fabricated by copper mould casting. In Journal of Physics: Conference Series (Vol. 266). Institute of Physics Publishing. https://doi.org/10.1088/1742-6596/266/1/012007