Fiber Characteristics and Mechanical Properties of Oxytenanthera abyssinica

7Citations
Citations of this article
12Readers
Mendeley users who have this article in their library.

Abstract

Unlike the culm hollow structure of most bamboo species, Oxytenanthera abyssinica has a unique solid or semi-solid culm, which may endow it with superior mechanical performance. In this study, the variation in fiber morphology and micro-mechanical properties across the radial regions of bamboo culm was examined by optical microscopy, scanning electron microscopy, X-ray diffraction, and nanoindentation. Results showed that the mean values of vascular bundle frequency and fiber tissue proportion were 1.76 pcs/mm (Formula presented.) and 21.04%, respectively, both of which increased gradually from inner to outer. The mean length, diameter, and length-diameter ratio of the fiber were 2.10 mm, 21.54 (Formula presented.) m, and 101.41 respectively. The mean indentation modulus of elasticity (IMOE) and hardness were 21.34 GPa and 545.88 MPa. The IMOE exhibited a significant increase from the inner to the middle region, and little change was observed from the middle to the outer region. There were slight fluctuations in hardness along the radial direction. The mean crystallinity and microfibril angle(MFA) of the fibers was 68.12% and 11.26 degrees, respectively. There is a positive correlation between cellulose crystallinity and the IMOE and hardness, while there is a negative correlation between the MFA and the IMOE and the hardness.

Cite

CITATION STYLE

APA

Yu, L., Dai, F., Zhang, K., Jiang, Z., Xia, M., Wang, Y., & Tian, G. (2023). Fiber Characteristics and Mechanical Properties of Oxytenanthera abyssinica. Plants, 12(16). https://doi.org/10.3390/plants12162987

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free