Characterization of electrospun novel poly(ester-ether) copolymers: 1,4-Dioxan-2-one and D,L-3-Methyl-1,4- dioxan-2-one

6Citations
Citations of this article
6Readers
Mendeley users who have this article in their library.

This article is free to access.

Abstract

Introduction: Because tissue engineering scaffolds serve as a temporary environment until new tissue can be formed, their mechanical performance, thermal properties, and biocompatibility are critical for maintaining their functionality. The goal of this study was to electrospin scaffolds from copolymers containing varying amounts of 1,4-Dioxan-2-one (DX) and D,L-3-Methyl-1,4-dioxan-2-one (DL-3- MeDX), and characterize their mechanical and thermal properties. Methods and Results: Image tool analysis of scanning electron micrographs revealed the presence of DL-3-MeDX causes the fiber diameter of the scaffold to decrease as compared to polydioxanone (PDO). Uniaxial tensile testing revealed increasing amounts of DL-3-MeDX in the copolymer decreases scaffold peak stress, strain at break and toughness. Modulated differential scanning calorimetry was used for thermal analysis of the scaffolds and showed that increasing amounts of DL-3-MeDX causes a decrease in the melting as well as crystallization temperatures. Conclusion: Based on the results of the mechanical and thermal properties of these copolymer scaffolds, it is evident that these constructs could be functional in a variety of biomedical engineering applications.

Cite

CITATION STYLE

APA

Wolfe, P. S., Lochee, Y., Jhurry, D., Bhaw-Luximon, A., & Bowlin, G. L. (2011). Characterization of electrospun novel poly(ester-ether) copolymers: 1,4-Dioxan-2-one and D,L-3-Methyl-1,4- dioxan-2-one. Journal of Engineered Fibers and Fabrics, 6(4), 60–69. https://doi.org/10.1177/155892501100600409

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free